PEX-B is made using a “Silane” or “Moisture Cure” method of cross-linking, where links between the molecules of the Polyethylene polymer are formed after the extrusion process using a catalyst and by exposing PEX tubing to water (steam bath) which creates HDPE (high-density polyethylene).